Carbides mei wear-resistant en corrosie-resistant
Beskriuwing
Excellent wear-resistant en corrosie-resistant coating materiaal, benammen geskikt foar wear-resistant beskerming yn fochtige sâlt spray omjouwing.Neffens de easken fan tsjinstprestaasjes wurde de pulverisearjende metoade en grûnstoffen oanpast om de bêste prestaasjes fan 'e coating te garandearjen.Applikaasje: wear ferset, fretting wear ferset, algemiene masines, alternative hurde chromium plating, soepeler oerflak, minder as fergees post machinin.
Spesifikaasje
Merk | Produkt Namme | Partikelgrutte (μm) | Skiekunde (wt%) | Type | Skynbere tichtens | Flowability | Eigenskippen | Oanfraach | |||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Co | C | Fe | W | Cr | B | Si | Ni | ||||||||
KF-65 | WC-10Co4Cr | 15-45, 10-38 | 9,5-10 | 5.3-5.6 | ≤0,8 | Bal. | 3,5-4,0 | Sinter & Crush | 5,5-6,5 g/cm3 | ≤25 s/50g | APS, HVOF, HVAF | Alternative hurde chromium plating;Petroleum, papier, algemiene masines | |||
KF-65 | WC-10Co4Cr | 15-45,10-38,5-30 | 9,5-10 | 5.3-5.6 | ≤0,8 | Bal. | 3,5-4,0 | Agglomerearre en sintere | 4,0-6,0 g/cm3 | ≤18 s/50g | APS, HVOF, HVAF | Alternative hurde chromium plating;Petroleum, papier, algemiene masines | |||
KF-65 | WC-10Co4Cr | 5-25, 5-15 | 9,5-10 | 5.3-5.6 | ≤0,8 | Bal. | 3,5-4,0 | Agglomerearre en sintere | 3,5-4,8 g/cm3 | Stabiele feeding oan poeder feeder | HVOF, HVAF | Alternative hurde ferchrooming; Gladder oerflak, minder as fergees postferwurking; | |||
KF-60 | WC-12Co | 15-45, 10-63 | 10.5-12 | 4.9-5.4 | ≤0,8 | Bal. | Sinter & Crush | 5,5-6,5 g/cm3 | ≤25 s/50g | APS, HVOF | Wear ferset, Fretting wear ferset | ||||
KF-60 | WC-12Co | 15-45, 10-38, 5-30 | 10.5-12 | 4.9-5.4 | ≤0,8 | Bal. | Agglomerearre en sintere | 4,0-6,0 g/cm3 | ≤18 s/50g | APS, HVOF, HVAF | Wear ferset, Fretting wear ferset, algemiene masines | ||||
KF-61 | WC-17Co | 15-45, 10-38 | 15.5-17 | 4.5-5.1 | ≤0,8 | Bal. | Agglomerearre en sintere | 3,5-5,5 g/cm3 | ≤25 s/50g | APS, HVOF, HVAF | Wear ferset, Fretting wear ferset, Better taaiens, algemiene masines | ||||
KF-62 | WC-25Co | 15-45, 10-38 | 22-26 | 4.0-4.6 | ≤0,8 | Bal. | Agglomerearre en sintere, Fertinking | 3,0-5,5 g/cm3 | ≤25 s/50g | APS, Detonation guns, kâlde spray | Fretting wear ferset, Better taaiens | ||||
KF-66 | WC-23%CrC-7Ni | 15-45, 10-38 | 6,0-6,8 | ≤0,8 | Bal. | 16.5-20 | 5,5-7 | Agglomerearre en sintere | 3,0-5,0 g/cm3 | ≤25 s/50g | APS, HVOF, HVAF | Alternative hurde chromium plating; Brûkt foar lege konsintraasje acid / alkali omjouwing by 200 ℃;Anti-oksidaasje en slijtbestriding by 750 ℃ | |||
KF-66 | 43WC-43%CrC-14Ni | 15-45,10-38 | 7,8-8,4 | ≤0,8 | Bal. | 35-38 | 12-14 | Agglomerearre en sintere | 2,0-4,0 g/cm3 | ≤35 s/50g | APS, HVOF, HVAF | Alternative hurde chromium plating Wurdt brûkt foar lege konsintraasje soer / alkali omjouwing by 200 ℃ | |||
KF-63 | WC-10Ni | 15-45,10-38 | 4,5-5,2 | ≤0.1 | Bal. | 8.5-10.5 | Agglomerearre en sintere | 4,0-6,0 g/cm3 | ≤18 s/50g | APS, HVF, HVAF | Net magnetyske wearbestindige coating.Better corrosie ferset | ||||
KF-70 | Cr3C2-25NiCr | 15-45, 20-53 | 9-11 | ≤1 | Bal. | 18-21.5 | Agglomerearre en sintere | ≥2,3 g/cm3 | Stabiele feeding oan poeder feeder | APS, HVOF | Anti-oksidaasje en wear ferset by 815 ℃ | ||||
KF-69 | Cr3C2-20NiCr | 15-45, 20-53 | 9-11 | ≤1 | Bal. | 15-17.5 | Agglomerearre en sintere | ≥2,3 g/cm3 | Stabiele feeding oan poeder feeder | APS, HVOF | Anti-oksidaasje en wear ferset by 815 ℃ | ||||
KF-71 | Cr3C2-30NiCr | 15-45, 20-53 | 9-11 | ≤1 | Bal. | 15-17.5 | Agglomerearre en sintere | ≥2,3 g/cm3 | Stabiele feeding oan poeder feeder | APS, HVOF | Anti-oksidaasje en wear ferset by 815 ℃.Better hurdens | ||||
KF-60 | WC-12Co (Low Carbon) | 15-45, 20-53 | 10.5-12 | 4.0-4.4 | ≤0,8 | Bal. | Agglomerearre en sintere | 4,0-6,0 g/cm3 | ≤18 s/50g | HVOF, HVAF | Wurdt brûkt foar Zn bad rollen yn Trochrinnende Galvanizing Lines | ||||
KF-68 | WC-30WB-10Co | 15-45,20-53,10-38 | 9-11 | 3,5-3,9 | Bal. | 1.4-1.7 | Agglomerearre en sintere | 3,0-4,9 g/cm3 | ≤30 s/50g | HVOF, HVAF | Wurdt brûkt foar Zn bad rollen yn Trochrinnende Galvanizing Lines | ||||
KF-68 | WC-30WB-5Co5Cr | 15-45,20-53,10-38 | 4-6 | 3,5-3,9 | Bal. | 4-6 | 1.4-1.7 | Agglomerearre en sintere | 3,0-4,9 g/cm3 | ≤30 s/50g | HVOF, HVAF | Wurdt brûkt foar Zn bad rollen yn Trochrinnende Galvanizing Lines | |||
KF-300E | 35% WC-NiCrBSi | 15-53,45-104 | 2,5-3,2 | 1.0-2.6 | 32-35 | 7,5-9 | 1,5-1,9 | 2.0-2.7 | Bal. | WC en NiCrBSi foarmjende alloy | 4,0-4,9 g/cm3 | ≤16 s/50g | HVOF, PS | Alternatyf Blended type WC + Ni60; Hegere materiaal gebrûk, leger enerzjyferbrûk, legere thermyske ynfloed; Brûkt foar glêsskimmel | |
KF-300F | 50% WC-NiCrBSi | 15-53,45-104 | 3.2-4.3 | 0,8-2,0 | 45-48 | 5.8-7.2 | 1,0-1,7 | 1,5-2,4 | Bal. | WC en NiCrBSi foarmjende alloy | 5,0-7 g/cm3 | ≤16 s/50g | HVOF, PS | Alternatyf Blended type WC + Ni60; Hegere materiaal gebrûk, leger enerzjyferbrûk, legere thermyske ynfloed; Brûkt foar glêsskimmel |